MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Morgan Advanced Ceramics Hilox ™ 991 Mac-A990S Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: A high purity, high quality alumina ceramic with an Al2O3 content in excess of 99%. An alumina grade developed for abrasive resistance and mechanical strength in chemically aggressive environments.

Prime Features:

  • Excellent resistance to corrosion and chemical attack
  • Exceptionally hard-wearing and abrasion resistant
  • Dense, non-porous and vacuum tight
  • Excellent dimensional stability across wide temperature range
Typical Applications:
  • Wear resistant components for rotary and reciprocating pumps handling chemically aggressive media: shafts, bearings, thrust washers, plungers, counterface seats.
Production Capabilities:
  • Complex components to close tolerances
  • Exacting flatness and surface finishes for low friction valve operation and accurate flow control
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: Mac-A990S
Vendors:
Available Properties
  • Density, fired
  • Open Porosity, fully dense, % nominal, apparent
  • Hardness, Rockwell HR45N
  • Flexural Strength, 3-point
  • Compressive Strength
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.