| KEBABLEND / MW 53.2000 PPS is a PPS-based product for the manufacture of soft magnetic components. The achievable permeability (µr) is about 15 and the saturation (Js) is 1130 mT. Properties: dimensionally stable, high continuous used temperature, semi-crystalline, soft magnetic Typical areas of application: Pumps and motors, Rotors Industries: Automotive, Electrical and electronics industry, Household appliances, Mechanical Engineering Information provided by BARLOG plastics GmbH. |