MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Zircar Ceramics DAHP Dense Alumina Hearth Plate
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity alumina. Designed for use as high load bearing members, they exhibit high strength at operating temperatures as high as 3400°F (1870°C). They are of exceptional high purity and contain only a trace of tramp oxides. 

Typical Applications:

  • Load bearing members in furnaces and thermal process systems operating as high as 3400°F (1870°C).
  • Hearth plates in rapid cycle furnaces with air atmospheres operating to 3317°F (1825°C).
  • Support plates in furnaces with hydrogen atmospheres operating over  3100°F (1700°C).
  • High temperature setters, supports and process fixtures.

Information provided by Zircar Ceramics.

Vendors:
Available Properties
  • Bulk Density
  • Porosity, Apparent
  • Permeability, g/s.Pa.m
  • Modulus of Elasticity
  • Modulus of Rupture
  • Modulus of Rupture
  • Modulus of Rupture
  • Compressive Strength, Crushing
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Emissivity (0-1)
  • Emissivity (0-1)
  • Emissivity (0-1)
  • Al2O3
  • Fe2O3
  • K2O+Na2O
  • Other, Other Oxides
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.