KEBABLEND / EC FE 170905 PPS is an electrically conductive PPS compound with carbon fiber reinforcement and graphite. Properties: antistatic, dimensionally stable, electrically conductive, good chemical resistance, good aging behavior, good fire behavior, high continuous used temperature, High strength, High stiffness, semi-crystalline Typical areas of application: Gears, Housing, Sliding elements, Plain bearing, Piston, Couplings, Bearing bushes, Pumps and motors, Pump housing, Sensors, Bobbin, Transport chains, Valves, Valve caps, Distributor Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Aviation Industry, Mechanical Engineering Information provided by BARLOG plastics GmbH. |