MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Pyrotek U-1 Compressible Board
Categories: Ceramic

Material Notes: U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free board is its ability to be formed to various shapes by wet molding. After drying its mechanical properties remain constant. U-1 is made from high-quality, shot free mineral wool and inert filters. It exhibits excellent flame and heat resistance with virtually no dimensional changes. It has self-cleaning properties and has no shot or abrasive elements to scratch hot glass.
Available forms
Boards: 1 m x 1 m
Boards: 40in x 40in

Available thickness
2.5 mm - 12 mm
3/32 in - 1/2 in

Applications

  • Glass lehr rolls
  • Gaskets and seals
  • Furnace lining
  • Catwalk insulation
  • Ball mill insulation
  • High-temperature compression gasket

Advantages

  • Asbestos-free
  • Excellent thermal stability
  • High mechanical strength
  • Non-abrasive
  • Wet moldable

Information provided by Pyrotek.

Vendors:
Available Properties
  • Density
  • Water Absorption at Saturation
  • Tensile Strength, Ultimate, ambient temperature
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Flexural Strength
  • Compressive Strength, 27%
  • Compressive Strength, 42%
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous
  • Shrinkage, Width
  • Shrinkage, Length
  • Shrinkage, Thickness
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Pyrotek, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.