Moplen HP3841 is a polypropylene homopolymer used for extrusion applications. Moplen HP3841 has a very narrow molecular weight distribution and is formulated with an anti-gasfading stabilization package. Moplen HP3841 is used for the production of continuous filaments. Typical applications are high tenacity yarns (HTY) and spunbond nonwovens. The grade being in development, this is a preliminary datasheet subjected to changes after product industrialization. This grade is not intended for medical and pharmaceutical applications. Status: Developmental Availability: Africa-Middle East; Asia-Pacific; Europe Application: Filament Yarn; Geotextile & Agriculture; Hygiene Nonwoven Market: Textile Processing Method: Continuous Filament/Spinning; Injection Molding; Spunbond Attribute: Homopolymer; Narrow Molecular Weight Distribution Information provided by LyondellBasell. |