MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond Supreme 45HT Toughened Heat Resistant Two Component Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: Key Features:
  • High temperature resistant
  • Superior thermal cycling capabilities
  • Excellent electrical insulator
  • Smooth and even flow properties
  • Very good peel strength
  • Exceptionally long working life
Product Description: Master Bond Supreme 45HT is a two component epoxy system featuring an attractive blend of superior physical properties especially shear and peel strengths for high performance structural bonding applications. It has a fine temperature resistance range of -100°F to +450°F. It is 100% reactive and does not contain any solvents or diluents. Supreme 45HT is distinctively formulated to withstand rigorous thermal cycling and for bonding dissimilar substrates. Supreme 45HT requires elevated temperature curing at a minimum of 250°F. The mix ratio is 100 to 30 by weight and is relatively forgiving. Supreme 45HT bonds well to similar and dissimilar substrates including metals, ceramics, glass, composites and many plastics and rubber materials. It withstands exposure to a variety of chemicals including water, many acids, bases, solvents, fuels and oils. It is a top notch electrical insulator. As mentioned previously, it is well conceived for bonding dissimilar substrates and withstands mechanical shocks and resists rigorous thermal cycling. The color of Part A is tan and the color of Part B is brown. Supreme 45HT would be most commonly used in aerospace, electronic and specialty OEM applications where excellent adhesion, top notch temperature resistance and splendid thermal cycling capabilities are required.

Product Advantages:

  • Non-critical 100 to 30 mix ratio by weight
  • Easily applied; smooth and even flow; contact pressure only required for cure
  • Exceptionally long pot life at room temperature
  • High bonding strength to similar and dissimilar substrates with very good peel strength
  • Exemplary thermal shock and cycling capabilities
  • Solid electrical insulation properties

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap, Aluminum to Aluminum
  • Peel Strength
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, followed by a post cure at 350-400°F for 1-2 hours
  • Cure Time
  • Working Life, After mixing, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.