MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chemours Viton® GFLT-600S with MgO Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Cures exceptionally fast to a high state of cure
  • Similar to improved low temperature properties compared to Viton® GFLT
  • Improved mold release/mold fouling properties
  • Improved mold flow and less shear sensitivity for a 65 Mooney peroxy cured FKM
  • Excellent physical properties with high elongation, both original and aged
  • Heat, fluids, and low temperature resistance comparable to Viton® GFLT
  • Improved water resistance/lower volume swell in water
  • Excellent compression set resistance with either low or no postcure

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors:
Available Properties
  • Hardness, Shore A, ASTM D1414, No Postcure
  • Hardness, Shore A, ASTM D1414, 2 hours Postcure
  • Hardness, Shore A, ASTM D1414, 4 hours Postcure
  • Tensile Strength at Break, ASTM D412, No Postcure
  • Tensile Strength at Break, ASTM D412, 4 hours Postcure
  • Tensile Strength at Break, ASTM D412, 2 hours Postcure
  • Tensile Stress at Strain, ASTM D412, No Postcure
  • Tensile Stress at Strain, ASTM D412, 2 hours Postcure
  • Tensile Stress at Strain, ASTM D412, 4 hours Postcure
  • Elongation at Break, ASTM D412, No Postcure
  • Elongation at Break, ASTM D412, 4 hours Postcure
  • Elongation at Break, ASTM D412, 2 hours Postcure
  • 100% Modulus, ASTM D412, No Postcure
  • 100% Modulus, ASTM D412, 2 hours Postcure
  • 100% Modulus, ASTM D412, 4 hours Postcure
  • Compression Set, ASTM D395B, O-Rings, postcured 2hrs
  • Compression Set, ASTM D395B, O-Rings, no postcure
  • Compression Set, ASTM D395B, O-Rings no postcure
  • Compression Set, ASTM D395B, O-Rings, postcured 2hrs
  • Glass Transition Temp, Tg, 2 hours Postcure
  • Processing Temperature, Cure
  • Processing Temperature, Postcure
  • Fluorine, F, Uncompounded Viton
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.