MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ExxonMobil Exxtra™ Adhere EAA8206HS Ethylene Acrylic Acid Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Product Description: Exxtra™ Adhere EAA8206HS resin is primarily intended for extrusion coating and coextrusion coating. It is the high draw down version of Exxtra™Adhere EAA8206 resin. It offers the following advantages: very low coating weight achievable at high line speed; very good adhesion to polarsubstrates, aluminum foil, metallized films, paper, iron, steel, and glass; and excellent balance of adhesion onto the substrates and interlayeradhesion with coextruded LDPE and EVA material.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Aluminum Containing Packaging
  • Coextrusion Coating
  • Cosmetic Packaging
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • Hygiene Packaging
  • Metalized Films

Information provided by ExxonMobil

Key Words: Escor™ 6000 ExCo
Vendors:
Available Properties
  • Density, ExxonMobil method
  • Acrylic Acid Content, ExxonMobil Method
  • Melt Flow, ASTM D1238
  • Neck In, ExxonMobil Method, 328 ft/min, constant output at 35 rpm
  • Neck In, ExxonMobil Method, 164 ft/min, constant output at 35 rpm
  • Neck In, ExxonMobil Method, 82 ft/min, constant output at 35 rpm
  • Drawdown, ExxonMobil Method, Constant output at 35 rpm
  • Melting Point, ExxonMobil method, Peak Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.