Pro-fax 7624 impact polypropylene copolymer is available in pellet form. This resin is typically used in extrusion applications and offers a very good stiffness/impact balance as well as an excellent resistance to aging at elevated temperatures in both wet and dry environments. Status: Commercial Availability: North America Application: Appliances; Automotive Parts; Interior Automotive Applications; Specialty Film; Underhood Market: Automotive; Flexible Packaging Processing Method: Blown Film; Sheet and Profile Extrusion; Tubing Attribute: Good Dimensional Stability; Good Heat Aging Resistance; Low Temperature Impact Resistance Information provided by LyondellBasell. |