Glass-filled Formlabs Rigid 4000 V.1 Resin prints with a smooth, polished finish, ideal for stiff, strong parts that can withstand minimal deflection. You can consider Rigid 4000 Resin for general load-bearing applications. The “4000” in the name represents the material’s tensile modulus. If you need a stiffer material, try Rigid 10K Resin. Supports print resolutions: 100 and 50 microns. Post-curing is required. Rigid 4000 Resin decreases the lifetime of resin tanks.
Information provided by Proto3000
|