MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Morgan Advanced Ceramics FireMaster® FireBarrier 135 Standard Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: FireMaster® FireBarrier products are cementitious materials designed for a variety of fire protection applications requiring strong and weather resistant exterior finishes.

Applications:

  • Tunnel fire protection (concrete linings, escape refuges, ventilation shafts)
  • A60 floating floors in ships

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density, dry
  • Density, long term
  • Density, installed
  • Modulus of Elasticity, after setting
  • Modulus of Elasticity, after 28 days
  • Compressive Strength, after 3 days curing, Cold Crushing Strength
  • Compressive Strength, after 3 days curing + drying, Cold Crushing Strength
  • Adhesive Bond Strength, ASTM E-736/06, on concrete surface
  • Adhesive Bond Strength, ASTM E-736/06, on steel surface
  • Specific Heat Capacity, EN 821-2
  • Specific Heat Capacity, EN 821-2
  • Specific Heat Capacity, EN 821-2
  • Thermal Conductivity, ISO 8302:1991
  • Thermal Conductivity, ISO 8302:1991
  • Thermal Conductivity, ISO 8302:1991
  • Maximum Service Temperature, Air
  • Al2O3
  • CaO
  • Fe2O3
  • Other, MgO+K2O+Na2O3
  • SiO2
  • TiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.