| High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracked composites, dies, fixtures, jigs, etc. Electrically non-conductive. Corrosion Resistance: resistant to most chemicals, solvents, acids and bases. |