| Product Description: Durable thin film nylon hybrid coating which provides extreme protection to the surfaces of internal components in aircraft cabins, cockpits and lavatories. Anti-Viral, Anti-Bacterial and Anti-Fungal. Electrically compatible. Excellent adhesion to metallic and nonmetallic substrates including previously coated materials, light alloys, rubbers, fabrics and glass. Prevents the transmission of pathogens on high contact surfaces.Information provided by: Nycote Laboratories Corporation |