MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
solder replacement adhesives
Johnson Matthey Easy-flo™ No. 25 Liquid Brazing Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Johnson Matthey Easy-flo™ No. 25 Liquid Flux is a liquid brazing flux suitable for use with silver brazing filler metals. It has a working range of 600-850°C and is suitable for use with filler metals melting below 800°C. Easy-flo™ No. 25 Liquid Flux formerly sold as Liquid Flux No. 25.

Easy-flo™ No. 25 Liquid Flux can be used for jewelry parts or any other application that requires the use of a liquid flux or where limited fluxing is required. This flux has also been used for brazing in furnaces that have poor atmospheres, where a flux is required to achieve filler metal wetting.

It can be used on precious metals as well as all of the common engineering materials (copper, brass, mild steel and stainless steel, but not aluminum). JM special purpose fluxes are required when brazing aluminum bronze, certain grades of stainless steel, tungsten, molybdenum and tungsten carbide or where protracted heating is involved.

Information provided by Johnson Matthey Metal Joining

Vendors:
Available Properties
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.