Key features:- Hardness: 85 - 90 Shore A
- Mixing ratio: 1:1 by volume
- 100% solid content
- Fast curing & easy to use
- No VOCs
Description: Polyurea coating system CPU-49-A100A-A/B is a fast-curing, polyurethane (polyurea series) MDI modified abrasion resistance flooring material; it begins by reacting an amine polyol with polyurea. It cures to form a elastic, flexible, abrasion resistance, high mechanical strength and dust resistance properties. It is waterproofing spray flooring coating which is suitable for most indoor floor, and can also be used as protective coatings. Application: - Application of office, classroom, hospital, equipment room, sanatorium floors, etc.
- Application of factories, food production, pharmaceutical production floors, Electronics manufacturer, etc.
- Application of supermarkets floors, department stores.
- Indoor or outdoor floors, waterproof parking lots.
- Indoor or outdoor aisles, square, stadiums waterproof floors, etc.
- Other indoor metal pipeline protective coatings.
Characteristics: - Abrasion resistance, durability and outstanding waterproofing properties.
- Seamless surface, decorative finish.
- No building restriction, easy application.
- Fast curing in 20 seconds; The surface can be walked, and will demonstrate the load-bearing property after 20 minutes of application.
Information provided by Taiwan PU Corporation |