Temper: Soft Anneal Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Butt Weld, Capacity for Being Hot Formed, Capacity for Being Cold Worked Common Fabrication Processes: Machining; Roll Threading and Knurling Typical uses: Terrazzo Strip; Fluid Connectors; Sensor Bodies; Thermostat Parts; Threaded Inserts for Plastic; Fittings; Hardware; Lock Bodies; Hot Combs (to Straighten Hair); Bolts; Screws; Adapters; Automatic Screw Machine Parts; Faucet Components; Fluid Connectors; Gauges; Gears; Nozzles; Pinions; Pneumatic Fittings; Screw Machine Products; Unions; Valve Seats; Valve Stems; Valve Trim; Faucet Seats; Plumbers' Brass Goods; Faucet Stems; Plumbing Fittings Applicable Specifications: Bar – SAE J461, AMS 4610; SAE J463, ASTM B16/B16M; Rod – SAE J463, AMS 4610, SAE J461, ASTM B16/B16M; Shapes – SAE J461, SAE J463, ASTM B16/B16M; Valves – MILITARY MIL-V-18436; Wire – ASTM B16/B16M |