MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Reynolds MT-13® Epoxy Adhesive Cement
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Overview: Smooth-On MT-13® is a premium performance epoxy for applications requiring maximum holding power and water resistance. MT-13® is a two component epoxy adhesive cement which is mixed in equal parts by volume (100A/123B by weight). Pot Life is 35 minutes and handling strength develops in 16 hours at 73° F / 23° C. MT-13® adheres extremely well to both porous and non-porous surfaces. MT-13® is widely used by the boating industry for assembly and general repair. MT-13® also maintains holding power under extreme cold conditions.

Information provided by Reynolds Advanced Materials

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Barcol, 935
  • Tensile Strength
  • Elongation at Break
  • Modulus of Elasticity, Compression
  • Modulus of Elasticity, Tension
  • Compressive Yield Strength
  • Adhesive Bond Strength, ASTM D1002, Exposure: None; Substrate: AL 2024-T-3
  • Adhesive Bond Strength, ASTM D1002, Exposure: None; Substrate: AL 2024-T-3
  • Adhesive Bond Strength, ASTM D1002, Exposure: None; Substrate: AL 2024-T-3
  • Adhesive Bond Strength, ASTM D1002, Exposure: 30 days in tap water @ 25°C; Substrate: AL 2024-T-3
  • Adhesive Bond Strength, ASTM D1002, Exposure: 7 days in 100% RH @ 65°C; Substrate: AL 2024-T-3
  • Adhesive Bond Strength, ASTM D1002, Exposure: None; Substrate: Cold Rolled Steel
  • Cure Time, Full Cure Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.