MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ineos K44-15-122 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF Standard 61 health effects requirements, and is recognized by the Plastic Pipe Institute as having a pipe material designation code of PE 3608 (formerly PE 3408). A pressure rated formulation is also produced when this product is extruded in combination with a Ineos approved black masterbatch. The resulting formulation known as K44-15-123 has NSF Standard 14 certification and complies with ANSI/NSF Standard 61 health effects requirements, is certified to CSA Standard B137.1-05 and B137.4-05, and is listed with the Plastic Pipe Institute as a PE 3608(formerly PE 3408) and PE 80 pipe material designation code.

Key Words: Natural PE 3608 pipe grade, meets ANSI/NSF Standard
Vendors:
Available Properties
  • Density, ASTM D4883, Natural
  • Environmental Stress Crack Resistance, ASTM D1693, Condition B
  • Environmental Stress Crack Resistance, ASTM D1693, Condition C
  • High Load Melt Index, ASTM D1238
  • PENT, ASTM F1473, Notch Tensile
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638, 2 in/min.
  • Tensile Strength, Yield, ASTM D638, 2 in/min.
  • Elongation at Break, ASTM D638, 2 in/min.
  • Flexural Modulus, ASTM D790, Secant-Method 1
  • Izod Impact, Notched, ASTM D256
  • Hydrostatic Design Basis, ASTM D2837
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Ineos Olefins & Polymers USA

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.