MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Polycasa XT Soft Tone PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: QUINN XT soft tone is an extruded acrylic sheet with the appearance and feel of traditional frosted glass but without the limitations of size and weight. QUINN XT soft tone offers a wide range of creative possibilities for building and industrial glazing, decoration, lighting and advertising, … thanks to its outstanding properties:
  • Improved light scatter
  • Stylish
  • trendy look
  • Avoids reflective effects
  • Easy to maintain, handle, fabricate and form
  • High light transmission
  • Good optical properties
  • Over lengths available
  • Stable thickness tolerances
  • Interior decoration
  • Information signs
  • Displays
  • Showcases
  • Shop fittings
  • Advertising signs
  • Advertising media

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors:
Available Properties
  • Transmission, Visible, Blue 019, single/double sided
  • Transmission, Visible, White 024,single/double sided
  • Transmission, Visible, Green 101, single/double sided
  • Transmission, Visible, Clear, single/double sided
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polycasa, formerly Quinn Group

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.