MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of flow characteristics. This epoxy has a 90 minute worklife and is a 1:1 mix ratio. Ideal for bulk application through meter mix dispensing equipment and the manufacture of large panel products.

Information provided by 3M

Vendors:
Available Properties
  • Brookfield Viscosity, Base, RVF #7 sp @ 20 rpm
  • Brookfield Viscosity, Accelerator, RVF #7 sp @ 20 rpm
  • Hardness, Shore D
  • Shear Strength, Overlap, Polycarbonate-IPA/abrade/IPA, Adhesive Failure
  • Shear Strength, Overlap, FRP(Green)-IPA/abrade/IPA, Cohesive Failure
  • Shear Strength, Overlap, FRP(Red)-IPA/abrade/IPA, Substrate Failure
  • Shear Strength, Overlap, Galvanized Steel-MEK/Abrade/MEK, Cohesive/Adhesive Failure
  • Shear Strength, Overlap, Al-MEK/Abrade/MEK, Cohesive Failure
  • Shear Strength, Overlap, Stainless Steel-MEK/Abrade/MEK, Cohesive/Adhesive Failure
  • Shear Strength, Aluminum, etched, Overlap, 30 day 65°C/80% RH, Cohesive Failure
  • Shear Strength, Overlap, CRS-MEK/Abrade/MEK, Cohesive/Adhesive Failure
  • Shear Strength, Aluminum, etched, Overlap, 30 day Gasoline soak, Cohesive Failure
  • Shear Strength, Aluminum, etched, Overlap, 30 day water soak, Cohesive Failure
  • Shear Strength, Aluminum, etched, Overlap, 30 day IPA soak, Cohesive Failure
  • Shear Strength, Aluminum, etched, Overlap, Control, Cohesive Failure
  • Shear Strength, Aluminum, etched, Overlap, Cohesive Failure
  • Shear Strength, Aluminum, etched, Overlap, Cohesive Failure
  • Shear Strength, Aluminum, etched, Overlap, Adhesive Failure
  • Shear Strength, Aluminum, etched, Overlap, Adhesive Failure
  • Shear Strength, Aluminum, etched, Overlap, Adhesive Failure
  • Peel Strength, ASTM D3167, Aluminum, etched, Bell Peel, Cohesive Failure
  • Peel Strength, ASTM D3167, Aluminum, etched, Bell Peel, Cohesive/Adhesive Failure
  • Peel Strength, ASTM D3167, Aluminum, etched, Bell Peel, Adhesive Failure
  • Cure Time, Time to Handling Strength
  • Cure Time, Full Cure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.