MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
ITW Insulcast® 502 Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST 502 is an unfilled epoxy with low viscosity for general purpose casting and impregnation, exhibiting excellent electrical and physical properties.

Information provided by ITW Performance Polymers.

Vendors:
Available Properties
  • Specific Gravity, Uncured. Insulcure 11B
  • Specific Gravity, Uncured. Insulcure 9
  • Specific Gravity, Uncured. Insulcast 502
  • Viscosity, ASTM D2392, Insulcure 9
  • Viscosity, ASTM D2393, Uncured, mixed. Insulcure 9
  • Viscosity, ASTM D2393, Uncured, mixed. Insulcure 11B
  • Viscosity, ASTM D2392, Insulcast 502
  • Viscosity, ASTM D2392, Insulcure 11B
  • Hardness, Shore D, ASTM D2240, cured. Insulcure 9
  • Hardness, Shore D, ASTM D2240, cured. Insulcure 11B
  • Tensile Strength, ASTM D638, cured. Insulcure 9
  • Tensile Strength, ASTM D638, cured. Insulcure 11B
  • Elongation at Break, ASTM D638, Cured. Insulcure 11B
  • Elongation at Break, ASTM D638, Cured. Insulcure 9
  • Flexural Strength, ASTM D790, Cured. Insulcure 9
  • Flexural Strength, ASTM D790, Cured. Insulcure 11B
  • Compressive Strength, ASTM D695, Cured. Insulcure 9
  • Compressive Strength, ASTM D695, Cured. Insulcure 11B
  • Volume Resistivity, ASTM D257, Insulcure 11B
  • Volume Resistivity, ASTM D257, Insulcure 9
  • Dielectric Constant, ASTM D150, Insulcure 11B
  • Dielectric Constant, ASTM D150, Insulcure 9
  • Dielectric Strength, ASTM D149, Insulcure 9
  • Dielectric Strength, ASTM D149, Insulcure 11B
  • Dissipation Factor, ASTM D150, Insulcure 11B
  • Dissipation Factor, ASTM D150, Insulcure 9
  • CTE, linear, Cured. Insulcure 11B
  • CTE, linear, Cured. Insulcure 9
  • Thermal Conductivity, Cured. Insulcure 11B
  • Thermal Conductivity, Cured. Insulcure 9
  • Maximum Service Temperature, Air, Insulcure 9
  • Maximum Service Temperature, Air, Insulcure 11B
  • Heat Distortion Temperature, Load Not Reported. Insulcure 9
  • Heat Distortion Temperature, Load Not Reported. Insulcure 11B
  • Pot Life, Insulcure 9. 100 grams
  • Pot Life, Insulcure 11B. 100 grams
  • Shelf Life, Insulcast 502
  • Shelf Life, Insulcure 11B
  • Shelf Life, Insulcure 9
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.