| Hostalen ACP 5331H B is a state of the art HDPE resin, produced by latest Hostalen ACP technology. Hostalen ACP 5331H B is easy processable on injection molding and compression molding equipment. Exceptional organoleptic properties and a good balance of stiffness, toughness and environmental stress cracking resistance make Hostalen ACP 5331H B the choice of customers for the production of beverages closures. It's also applicable for many other types of food and nonfood caps and closures, as well as tube shoulders. Availability: Asia-Pacific Application: Caps & Closures; Collapsible Tubes Market: Consumer Products; Rigid Packaging Processing Method: Compression Molding; Injection Molding Attribute: Good ESCR (Environmental Stress Cracking Resistance); Good Organoleptic Properties; Good Toughness; High Density Information provided by LyondellBasell. |