MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SABIC SABIC® LLDPE 318BJ PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE 318BJ is a butene linear low density polyethylene resin typically designed for easy processing and specially formulated for optimum thermal stability at high temperatures used in cast film extrusion. Cast film produced from SABIC® LLDPE 318BJ exhibit excellent optical properties, puncture resistance and tear strength .SABIC® LLDPE 318BJ is TNPP free. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ISO 868, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Tensile Strength at Break, ASTM D638, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Tensile Strength, Yield, ASTM D638, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Elongation at Break, ASTM D638, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Elongation at Yield, ASTM D638, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Flexural Modulus, 1% Secant, ASTM D790, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Puncture Energy, ASTM D5748-95, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Tear Strength, ISO 6383-2, TD; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Dart Drop Total Energy, ISO 7765-2, Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, 2000 V/sec
  • Dissipation Factor, ASTM D150
  • Melting Point, SABIC method
  • Vicat Softening Point, ISO 306, at 10 N (VST/A)
  • Haze, ASTM D1003, 2.5 BUR using 100% 318BJ.
  • Gloss, ASTM D2457, 45°; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 318BJ.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.