MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Reynolds Smooth-Cast® 385 Mineral Filled Urethane Casting Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Smooth-Cast™ 385 is a mineral filled urethane casting resin that is very hard and durable. When Parts A and B are mixed in proper proportion (1A:5B by weight), Smooth-Cast™ 385 cures at room temperature with virtually no shrinkage. This rigid urethane casting resin has high compressive and flexural strength. Fully cured castings are tough, machinable and paintable. Color effects are possible by adding pigment dispersions. They resist moisture and mild solvents. Smooth-Cast™ 385 is ideal for making industrial production parts, foundry patterns, vacuum forming molds, and some ceramic applications.

Information provided by Reynolds Advanced Materials

Vendors:
Available Properties
  • Specific Gravity, ASTM D-1475
  • Viscosity, ASTM D-2393, Mixed
  • Linear Mold Shrinkage, ASTM D-2566
  • Hardness, Shore D, ASTM D-2240
  • Tensile Strength, Ultimate, ASTM D-638
  • Elongation at Break, ASTM D-638
  • Tensile Modulus, ASTM D-638
  • Flexural Strength, ASTM D-790
  • Flexural Modulus, ASTM D-790
  • Compressive Strength, ASTM D-695
  • Compressive Modulus, ASTM D-695
  • Heat Distortion Temperature, ASTM D-648
  • Cure Time, Handling Time
  • Pot Life, ASTM D-2471
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.