MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Baystarâ„¢ HL 323 MDPE Medium Density Polyethylene, Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Medium molecular weight, medium density film resin

Characteristics:

  • Excellent balance of stiffness and impact strength
  • Good puncture resistance
  • Excellent compatibility with LDPE and LLDPE
  • Good tensile strength

Applications:

  • Specialty Merchandise bags
  • Mailing envelopes
  • Heavy-duty shipping sacks
  • Pallet shrink films
  • Fresh cut produce packaging
  • Coextrusion
Film was produced at 1.0 mil with a 2.5:1 BUR

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Key Words: Excellent balance of stiffness and impact strength
Vendors:
Available Properties
  • Density, ASTM D-792
  • Water Vapor Transmission, ASTM F1249, 90%RH
  • Melt Flow, ASTM D-1238
  • Film Tensile Strength at Yield, MD, ASTM D-882, A
  • Film Tensile Strength at Yield, TD, ASTM D-882, A
  • Film Elongation at Break, MD, ASTM D-882, A
  • Film Elongation at Break, TD, ASTM D-882, A
  • Elmendorf Tear Strength MD, ASTM D1922
  • Elmendorf Tear Strength TD, ASTM D1922
  • Dart Drop Test, ASTM D-1709, A
  • Film Tensile Strength at Break, MD, ASTM D-882, A
  • Film Tensile Strength at Break, TD, ASTM D-882, A
  • 1% Secant Modulus, MD, ASTM D-882, A
  • 1% Secant Modulus, TD, ASTM D-882, A
  • Melting Point, ASTM D-3417
  • Haze, ASTM D1003
  • Gloss, ASTM D2457
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.