MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman Cristal™ EB062 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ EB062 copolyester is a resin specifically developed for extrusion-blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand particularly in packaging for cosmetics and personal care. Compared to commonly used materials, Cristal EB062 runs on most standard processing equipment. Extremely high melt strength makes the resin an excellent choice when manufacturing bottles. This product offers improved toughness, melt strength, chemical resistance, excellent color, and clarity in thick-walled applications. Cristal EB062 is certified to NSF/ANSI Standard 51 for Food Equipment Materials. Cristal™ EB062 is cleared for various food contact applications (including contact with most alcoholic beverages) by FCN No. 1234 as described in the Food and Drug Administration (FDA) Inventory of Effective Food Contact Substance Notifications and may be used in full compliance with the United States Federal Food and Drug, and Cosmetic Act, provided that it is used within the limitations set forth for FCN 1234

Applications

  • Bottles-skin care pkg
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Skin care packaging
Key Attributes
  • Easy to extrude, cut, print, and seal
  • Effective barrier properties
  • Excellent chemical resistance
  • Excellent clarity
  • Excellent colorability
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Toughness

Information provided by Eastman.

Vendors:
Available Properties
  • Density, ASTM D792
  • Linear Mold Shrinkage, ASTM D955
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched, ASTM D4812
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003
  • Transmission, Visible, ASTM D1003, Regular
  • Transmission, Visible, ASTM D1003, Total
  • FDA, See notes for details
  • NSF Compliance, See notes for details
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.