MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Go Yen Chemical Rutile Type Paint & Coating Titanium Dioxide TIO2
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Paint & coating grade tio2 ofers excellent weather resistant for all kinds of materials, and used in exterior and interior products. Excellent blue toner makes Paint & coating gradet tio2 can apply into products with high required for color and dispersing, such as master batch, ink, and pigment.

Advantages:

  • high whiteness
  • Weather resistance
  • Special nano surface treatment
  • Excellent opacity
  • Good hiding power
  • Distribution concentrated particle size
  • Good coloring force
  • Excellent dispersion performance
  • Excellent durability
  • Hue bluish tone
Applications:
  • Polyvinyl chloride (indoor and outdoor)
  • Wide range of water-based paint and oil paint
  • Powder coatings and industrial paints
  • PP.PE.EVA.PVC and polyolefin products
  • Engineering plastics
  • Thermoplastic products
  • EMC, melamine, PU, unsaturated resin
  • Natural rubber and synthetic rubber
  • Printing ink, pigment, masterbatch
  • General Plastics, rubber, resin, and various polymers
  • Wide range of other industrial applications

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Brightness, Whiteness
  • Oil Absorption
  • Particle Size, Sieve residue ?0.01%
  • pH
  • TiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.