MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik Polymer VS 2500
Categories: Polymer

Material Notes: The products of the Polymer VS series are vinyl-terminated polydimethyl siloxanes with different viscosity levels and molecular weights, and an extremely low content of volatile constituents. They serve as a base polymer in addition-crosslinking silicone formulations. Polymer VS is also available in viscosities other than those listed below.

Application: Polymer VS cures by a platinum-catalyzed addition reaction with silicone crosslinkers containing SiH groups. Due to the low content of volatile constituents and the crosslinking mechanism, the curing shrinkage remains low and no volatile or corrosive substances are formed while curing. Polymer VS can be used for a wide range of applications by selecting the suitable crosslinkers (Crosslinker 100 series, Crosslinker 200 series), catalysts (Catalyst 500 series), additives and fillers (VQM, Compound VS).

Information provided by Evonik

Vendors:
Available Properties
  • Volatiles
  • Viscosity
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.