MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Fluorseals PTFE Unfilled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes:

Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.

Vendors:
Available Properties
  • Density, DIN 53479
  • Deformation, ASTM D621-59, 14 MPa, 100 h, 23°C
  • Hardness, Shore D, DIN 53505
  • Ball Indentation Hardness, DIN 53456
  • Tensile Strength at Break, ASTM 1457-69 T
  • Elongation at Break, ASTM 1457-69 T
  • Tensile Modulus, DIN 53457
  • Flexural Strength, DIN 53452, 3.5% Flexural Stress
  • Compressive Yield Strength, DIN 53454, 1% Yield Point
  • Compressive Yield Strength, DIN 53454, 10% Yield Point
  • Izod Impact, Notched (ISO), DIN EN ISO 197 397
  • Izod Impact, Unnotched (ISO), DIN EN ISO 197 397
  • Coefficient of Friction, Dynamic, v = 1 m/s
  • Coefficient of Friction, Dynamic, v = 1.9 m/s
  • Abrasion, Partner Material ST 50, mm of depth after 5 hrs load duration
  • Torsional Stiffness, DIN 53447
  • Volume Resistivity, DIN 53482
  • Surface Resistance, DIN 53482
  • Dielectric Constant, DIN 53483
  • Dielectric Strength, VDE 0303 Part 2
  • Dissipation Factor, DIN 53483
  • Dissipation Factor, DIN 53483
  • Dissipation Factor, DIN 53483
  • Dissipation Factor, DIN 53483
  • Comparative Tracking Index, VDE 0303 Part 1/9.64
  • CTE, linear, DIN 52328
  • CTE, linear, DIN 52328
  • CTE, linear, DIN 52328
  • Specific Heat Capacity, adiabatic calorimeter
  • Specific Heat Capacity, adiabatic calorimeter
  • Thermal Conductivity, DIN 52612
  • Melting Point, DTA, Melting Range
  • Maximum Service Temperature, Air, Long Term
  • Maximum Service Temperature, Air, Short Term
  • Vicat Softening Point, DIN 53460, in air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.