MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SSAB Docol S900MC Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: The high-strength structural steel SSAB Docol S900MC is a hot-rolled steel made for cold forming, with a minimum yield strength of 900 MPa. SSAB Docol S900MC meets or exceeds the requirements of S900MC in EN 10149-2. SSAB Docol S900MC is provided as cut-to-length sheets with excellent thickness accuracy and surface quality. Typical applications include a wide range of components and parts for lighter transport solutions.

Dimension Range: SSAB Docol S900MC is available as cut to length sheets with mill edge in thicknesses of 3.00 - 10.00 mm, widths up to 1600 mm and lengths up to 13 meters.

Data provided by SSAB.

Vendors:
Available Properties
  • Tensile Strength, Rm
  • Tensile Strength, Rm
  • Tensile Strength, Yield, ReH
  • Tensile Strength, Yield, ReH
  • Elongation at Break, A5
  • Elongation at Break, A5
  • Charpy Impact, 10x10 mm, longitudinal
  • Bend Radius, Minimum, Inner bending radius for a 90° bend, Logitudinal
  • Bend Radius, Minimum, Inner bending radius for a 90° bend, Logitudinal
  • Carbon, C
  • Iron, Fe, Balance
  • Manganese, Mn
  • Niobium, Nb (Columbium, Cb)
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.