MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP21LSCL-2 Two component epoxy for bonding, coating, sealing and potting
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Low viscosity
  • Long working life
  • Good physical strength properties
  • Excellent electrical insulation properties
Master Bond EP21LSCL-2 is a two component, low viscosity epoxy resin system featuring superb optical clarity. This system has a forgiving mix ratio of 100 to 20 by weight. The recommended cure schedule is overnight at room temperature followed by 3-5 hours at 140-175°F. It has exceptionally low exotherm and a long working life of 6 to 8 hours for a 100 gram mass. This compound is 100% reactive and does not contain any solvents or diluents.EP21LSCL-2 bonds well to a wide variety of substrates including metals, glass, composites, ceramics as well as many rubber and plastic materials. It is a superb electrical insulator. When this property is combined with its low exotherm, it enables EP21LSCL-2 to be highly effective in larger potting and encapsulation applications. The system’s most outstanding feature is its non yellowing characteristic. EP21LSCL-2 is specially formulated to have minimal non-yellowing tendencies. It is a very good adhesive with low shrinkage upon curing and exceptional dimensional stability. It is resistant to water, oils, fuels and outdoor elements. The service temperature range is from -60°F to +250°F. EP21LSCL-2 is an attractive option when

Product Advantages:

  • Low viscosity; easy to apply or pour
  • Contains no solvents or diluents
  • Low shrinkage upon curing
  • Long open time
  • Highly desirable non-yellowing profile
  • Meets NASA low outgassing specifications

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Mixed
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap Shear; Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Refractive Index
  • Cure Time, Optimum cure schedule: Overnight at room temperature followed by 3-5 hours at 140-175°F
  • Working Life, After mixing, 100 gram batch
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.