Pro-fax SV152 is a nucleated, very high impact polypropylene copolymer available in pellet form. This resin is typically used in general extrusion and blow molding applications and offers excellent cold temperature impact resistance. ASTM and ISO-based versions of the technical data sheet are available for Pro-fax SV152. Availability: North America Application: Automotive Parts; Corrugated Sheet; Opaque Containers Market: Automotive; Rigid Packaging Processing Method: Extrusion Blow Molding; Sheet; Sheet and Profile Extrusion; Thermoforming Attribute: Good Stiffness; Low Temperature Impact Resistance; Nucleated Information provided by LyondellBasell. |