MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Bynel® 3126 Adhesive Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins

Applications:Bynel® 3126 adheres to a wide variety of materials. It is most often used to adhere to PE, acid copolymers, and ionomers. The use of Bynel® Series 3100 resins can be advantageous in applications where acid-containing polymers, such as acid copolymers or ionomers, are to be combined with PVDC.

Bynel® Series 3100 resins can be used in coextrusion processes including:

  • blown film
  • cast film/sheet
  • extrusion coating
  • thermal lamination
  • Physical properties Bynel® Series 3100 resins are typical of EVA resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others for a particular extrusion process.

    Information provided by DuPont™

    This former DuPont product line is now a Dow product line.

    Vendors:
    Available Properties
    • Density, ASTM D792
    • Melt Flow, ASTM D1238
    • Melting Point, ASTM D3418, Freezing Point, DSC
    • Melting Point, ASTM D3418, DSC
    • Vicat Softening Point, ASTM D1525
    • Rear Barrel Temperature
    • Middle Barrel Temperature
    • Front Barrel Temperature
    • Adapter Temperature
    • Die Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Dow Chemical (former DuPont)

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Visit Zeus Inc. for PEEK Tubing
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.