MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Versalis Clearflex® MQ F0 Very Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Very Low Density Polyethylene (VLDPE)

Material Notes: Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).

The resin shows an excellent balance between flexibility and impact resistance.

Main Applications: Clearflex MQ F0 is suitable for injection molding. Products made with Clearflex MQ F0 are characterized by a high flexibility. Clearflex MQ F0 is recommended for seals and gaskets, for blend with polyolefins to modify and improve impact resistance.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Melt Flow, ISO 1133
  • Hardness, Shore D, ISO 868/A
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Flexural Modulus, ISO 178
  • Melting Point, Internal method
  • Vicat Softening Point, ISO 306/A
  • Brittleness Temperature, ASTM D746
  • Transmission, Visible, clear; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polimeri Europa (Former Polimeri Europa (EniChem)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.