| Hostacom TRC 483N NA 5J2F Speck is a 19% talc-reinforced TPO with speckled effect fibers for automotive interior injection molding applications. It has a strong balance of impact and stiffness, UV stability, and high scratch resistance. This grade is for molding decorative interior parts, such as door trim panels, that require strong impact resistance, stiffness, and resistance to scratching and marring. Hostacom TRC 483N NA grades are available in the natural resin color or color-matched with various OEM colors. Availability: North America Application: Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Excellent Processability; High Impact Resistance; High Rigidity; Scratch Resistant; UV Stabilized Information provided by LyondellBasell. |