| Emulprene 1783 is a copolymer styrene – butadiene cold emulsion polymerized used fatty and rosin acid as emulsifier, coagulated by salt-acid system and it is extended utilizing 37.5 phr of RAE (Residual Aromatic Extract). Uses: Emulprene 1783 is used in the manufacture of tires, retreading, conveyor belts, hoses, mechanical goods for its excellent processing properties. Information provided by Dynasol Group. |