| A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent machining and tensile properties at room temperature. A-706 is qualified under Mil. Spec. MMM-A-134, Type III. Information provided by Ellsworth Adhesives. |