MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chemours 350 PFA Perfluoroalkoxy Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Combines the processing ease of conventional thermoplastic resins with the excellent properties of PTFE. High chemical resistance, superior electrical properties, high service temperatures, superior high temperature creep resistance, excellent low temperature toughness, and exceptional flame resistance. Processed by conventional melt-extrusion and molding techniques. Resin Characteristics: Premium resin with enhanced ESCR. Lowest flow rate of this series. Uses: Films; chemical linings; transfer-molded articles; tubing.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015. This specific product was discontinued prior to the formation of Chemours.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570, 24 hours
  • Melt Flow, ASTM D3307
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D3307
  • Tensile Strength, Ultimate, ASTM D3307
  • Tensile Strength, Ultimate, ASTM D1780
  • Tensile Strength, Yield, ASTM D3307
  • Elongation at Break, ASTM D3307
  • Elongation at Break, ASTM D1708
  • Elongation at Break, ASTM D3307
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Compressive Modulus, ASTM D695
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256-72a
  • Coefficient of Friction, Dynamic, 3 ft/min; 100 psi; dry vs. steel
  • Coefficient of Friction, Dynamic, 10 ft/min; 100 psi; dry vs. steel
  • Coefficient of Friction, Dynamic, 30 ft/min; 100 psi; dry vs. steel
  • Coefficient of Friction, Dynamic, 50 ft/min; 100 psi; dry vs. steel
  • K (wear) Factor, 50 ft/min; 100 psi; dry vs. steel
  • K (wear) Factor, 30 ft/min; 100 psi; dry vs. steel
  • K (wear) Factor, 3 ft/min; 100 psi; dry vs. steel
  • K (wear) Factor, 10 ft/min; 100 psi; dry vs. steel
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Short time
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • CTE, linear, ASTM D696
  • CTE, linear, ASTM D696
  • CTE, linear, ASTMD 696
  • Specific Heat Capacity
  • Melting Point, ASTM D3418
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, Glass II
  • Glass Transition Temp, Tg, Glass I
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Refractive Index, ASTM D542-50
  • Haze, ASTM D1003-52
  • Transmission, Visible, 0.40 to 0.70 µm
  • IR Transmittance, 0.70 to 2.40 µm, 2.5%
  • UV Transmittance, 0.25 to 0.70 µm
  • Processing Temperature, Cure Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.