Description: Delrin® 510MP is a medium viscosity grade containing 10% Teflon® Micropowder.
Applications: It is designed for applications requiring moderate low 2wear and friction against steel, itself, or other plastics.
Specifications: Mechanical properties measured at 23°C unless otherwise stated.
Comments: Processing Moisture Content: 0.2% Max.
Data provided by DuPont Engineering Polymers for the Americas region.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPOM, Polyoxymethylene