MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
GEHR Plastics PBT® Polybutylene Trephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Extremely high toughness allows the use of self tapping screws or inserts. The good sliding properties and the high dimensional stability also open up a wide range of possible applications. Very good results can be achieved in joining processes with two component adhesives on the basis of e.g. epoxy resins or cyanoacrylates as well as silicones. Painting of the part or high vacuum coating of the component surface is also possible. The continuous operating temperature ranges from approx. -60°C to 100°C. Properties: high stability, stiffness and toughness even at low temperatures, good creep resistnac, high surface hardness, good polishability, high dimensional stability, easy to metalize, good sliding proerties, good electrical insulation characteristics, high resistnace to chemicals, easy to paint, good UV and weather resistance, sensitive to hydrolysis. Applications: components with metal inserts, pump components, housing components, tankk caps, gear wheels, insulation parts in electrical engineering, applications with UV exposure.

information provided by GEHR

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Moisture Absorption at Equilibrium, ISO 62
  • Water Absorption at Saturation, ISO 62
  • Ball Indentation Hardness, ISO 2039
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Strength, ISO 178
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • CTE, linear, ISO 11359
  • Melting Point, DIN EN ISO 3146
  • Maximum Service Temperature, Air, UL 746B
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Vicat Softening Point, ISO 306, VST/A/50
  • Vicat Softening Point, ISO 306, VST/B/50
  • Minimum Service Temperature, Air, UL 746B
  • Glass Transition Temp, Tg, DIN EN ISO 3146
  • Flammability, UL94, UL 94, test results without UL registration
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GEHR Plastics Inc

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.