| Hostacom TRC 787N D E is a 20% talc filled PP copolymer, with excellent impact/stiffness balance, good processability, high scratch resistance and good surface appearance. This grade is delivered in customer customized colors. The product is available in G91428 color version, pellet form. This product is also available in other colors, new colors can be developed depending on customer requirements. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts; Interior Automotive Applications; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Antistatic; Ductile; Good Abrasion Resistance; Good Color Stability; Good Processability; Good Stiffness; Good Surface Finish; High Flow; High Impact Resistance; Low Density; Low Temperature Impact Resistance; Low to No Odor; Low VOC Emission; Pleasing Surface Appearance; Scratch Resistant; UV Resistant Information provided by LyondellBasell. |