MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
solder replacement adhesives
Lucas-Milhaupt Silvaloy® A34T Brazing Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy A34T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult wet metals such as stainless steel and tungsten carbide. This alloy, being free of Pb or Cd is preferred for long heating cycles and is suitable for use in controlled atmosphere brazing without flux. The largest use of this alloy is for furnace brazing although it is also suitable for other brazing procedures. Typical applications are the joining of ferrous, nonferrous, and dissimilar metals and alloys with close joint clearances.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Key Words: EN 1044 AG 106
Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Electrical Resistivity
  • Melting Point
  • Solidus
  • Liquidus
  • Maximum Service Temperature, Air, continuous
  • Maximum Service Temperature, Air, intermittent
  • Processing Temperature, Brazing Temperature
  • Copper, Cu
  • Other, total
  • Silver, Ag
  • Tin, Sn
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lucas-Milhaupt Warwick, LLC, formerly Wolverine Joining Technologies

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.