MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Lord Adhesives CoolTherm™ SC-252 Silicone encapsulant system
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: LORD CoolTherm™ SC-252 thermally conductive silicone encapsulant is a two-component system designed to provide excellent thermal conductivity for electrical/electronic encapsulating applications, while retaining desirable properties associated with silicones. CoolTherm SC-252 encapsulant can be either room temperature cured or heat cured for maximum adhesion.

Features: exhibits low shrinkage and stress on components as it cures. maintains low viscosity for ease of component encapsulation compared to other highly thermally conductive materials. provides high thermal conductivity for applications where superior heat dissipation is required. composed of an addition-curing polydimethyl siloxane polymer that will not depolymerize when heated in confined spaces. provides excellent thermal shock resistance.

All information provided by Lord.

Vendors:
Available Properties
  • Specific Gravity, SC-252 Resin
  • Specific Gravity, Mixed
  • Specific Gravity, SC-252 Hardener
  • Viscosity, SC-252 Hardener, 10s^-1 Shear Rate
  • Viscosity, SC-252 Resin, 10s^-1 Shear Rate
  • Viscosity, mixed, 10s^-1 Shear Rate
  • Hardness, Shore A, ASTM D 2240, cured
  • Tensile Strength
  • Volume Resistivity, ASTM D 257, cured
  • Dielectric Constant, ASTM D 150, cured
  • Dissipation Factor, ASTM D 150, cured
  • Thermal Conductivity, Hot Disc Transient Method, cured
  • Working Life, Mixed
  • Gel Time, mixed
  • Shelf Life, each component from date of manufacture
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.