MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
VICTREX ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetherketoneetherketoneketone (PEKEKK), Wear Resistant

Material Notes: Product Description:

High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, color natural/beige.

Typical Application Areas:

Applications for high strength and stiffness as well as good ductility at higher temperatures. Chemically resistant to aggressive environments.

Information Provided by Victrex.

Key Words: PEKEKK
Vendors:
Available Properties
  • Density, ISO 1183, Crystalline
  • Water Absorption at Saturation, ISO 62-1
  • Viscosity, ISO 11443, melt
  • Linear Mold Shrinkage, Flow, ISO 294-4, 395°C nozzle, 200°C tool
  • Linear Mold Shrinkage, Flow, ISO 294-4, 415°C nozzle, 220°C tool
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 395°C nozzle, 200°C tool
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 415°C nozzle, 220°C tool
  • Spiral Flow, Mold Temp: 200°C, Melt Temp: 395°C
  • Spiral Flow, Mold Temp: 220°C, Melt Temp: 415°C
  • Spiral Flow, Mold Temp: 200°C, Melt Temp: 395°C
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Unnotched (ISO), ISO 180/U
  • Charpy Impact Unnotched, ISO 179/1U
  • Charpy Impact, Notched, ISO 179/1eA
  • Volume Resistivity, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, Parallel to Flow, ISO 11359, Below Tg
  • CTE, linear, Parallel to Flow, ISO 11359, Above Tg
  • CTE, linear, Transverse to Flow, ISO 11359, Below Tg
  • CTE, linear, Transverse to Flow, ISO 11359, Above Tg
  • Thermal Conductivity, ISO 22007-4, Along flow
  • Thermal Conductivity, ISO 22007-4, Average
  • Melting Point, ISO 11357
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-f
  • Glass Transition Temp, Tg, ISO 11357, Onset
  • Glass Transition Temp, Tg, ISO 11357, Midpoint
  • Mold Temperature
  • Drying Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.