MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SABIC SABIC® LDPE PCG22 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE grades for healthcare applications are produced under controlled conditions resulting in high product quality, consistency and a high level of purity. SABIC® LDPE PCG22 is an additive free grade, typically designed for healthcare packaging and can typically be converted by Injection Molding to produce caps and closures. It exhibits a high MFR for good flow properties. Compliance to Regulations SABIC® LDPE PCG22 complies with the relevant monographs of the European Pharmacopoeia (EP) and the United States Pharmacopoeia (USPVI).

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133, ml/10 min
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133, ml/10 min
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527-2, Test specimen according to ISO 527-2 type 1BA, thickness 2 mm,Speed of testing: 50 mm/min
  • Tensile Strength, Yield, ISO 527-2, Test specimen according to ISO 527-2 type 1BA, thickness 2 mm,Speed of testing: 50 mm/min
  • Elongation at Break, ISO 527-2, Test specimen according to ISO 527-2 type 1BA, thickness 2 mm,Speed of testing: 50 mm/min
  • Creep Strength, ISO 899, Modulus; Determined at 23 °C, 3 MPa,Test specimen according to ISO 3167, thickness 4 mm
  • Creep Strength, ISO 899, Modulus; Determined at 23 °C, 3 MPa,Test specimen according to ISO 3167, thickness 4 mm
  • Tensile Modulus, ISO 527-2, Test specimen according to ISO 527-2 type 1BA, thickness 2 mm,Speed of testing: 50 mm/min
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Notched (ISO), ISO 180/A
  • Heat of Fusion, DIN 53765
  • Melting Point, DIN 53765
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2, Conditioning of test specimen: temp. 23 °C, relative humidity 50 %, 24 hours
  • Vicat Softening Point, ISO 306, at 10 N (VST/A)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.