MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Clyrell EC 2340 Polypropylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell EC2340 is an heterophasic copolymer. It does not contain slip or anti-blocking additives. Clyrell EC2340 is typically used for the extrusion of films for food packaging, lamination, labeling films, thermoformed containers, stationery and protective films. The films produced with Clyrell EC2340 have been reported by customers to exhibit a good balance of toughness and mechanical properties, very good optical properties, easy processing and low stress whitening. Customers also reported that Clyrell EC2340 may not require coextrusion with random copolymers to obtain a good clarity film. Applications: Bags & Pouches, Food Packaging Film, Lamination Film

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Melt Flow, ISO 1133-1
  • Tensile Strength at Break, ISO 527-1,-2
  • Tensile Strength, Yield, ISO 527-1,-2
  • Elongation at Break, ISO 527-1,-2
  • Elongation at Yield, ISO 527-1,-2
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179-1/1Ea
  • Charpy Impact, Notched, ISO 179-1/1Ea
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1,-2, unannealed
  • Vicat Softening Point, ISO 306, A50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.