MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Momentive Performance Materials Silopren™ LSR 4080 Liquid Silicone Rubber - Healthcare
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding process allows for complex part geometry and exact dimensions. LSR elastomers are generally suitable for short cycle time injection and full automatic flash-less processing. Color pastes are available to pigmenting addition cure productions of LSR's.

All LSR grades are platinum cured materials which are mixed in a 1:1 ratio by weight.

The distinctive properties of silicone elastomers - purity, clarity, strength - coupled with ease of processability, have resulted in their use in a broad range of medical device applications. Silicone materials exhibit exceptional stability over a wide range of temperatures, lending themselves to use in applications requiring repeated sterilization performance.

Typical applications include, but are not limited to:

  • Dental / surgical devices
  • Diagnostics / imaging
  • Fluid and drug delivery devices
  • Orthopedics / prosthetics
  • Scar management
  • Septa / stoppers / laboratory accessories
  • Medical tubing
  • Wound drains and bulbs
  • Sterilization mats
  • Pharmaceutical closures
  • Instrument grips
  • Dialysis o-rings
  • Positioning devices
  • Catheters
  • Seals / o-rings / valves
  • Respiratory / anesthesia
  • Medical equipment keypads

Vendors:
Available Properties
  • Specific Gravity
  • Linear Mold Shrinkage, vulcanized 10 sec at 200°C; Without post-cure
  • Linear Mold Shrinkage, vulcanized 10 sec at 200°C then post-cured
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Tear Strength, Die B
  • Compression Set, Post cured
  • Transmission, Visible, transparent; thickness unknown
  • Nozzle Temperature, cool nozzle and cylinder to prevent premature vulcanization
  • Mold Temperature, short vulcanization time required (a few seconds)
  • Injection Pressure, depends on feed channel
  • Hold Pressure
  • FDA, FDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Momentive Performance Materials (GE Silicones)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.