MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Solvay MTM® 79 Epoxy Matrix with 50% CF1420 Carbon Fiber Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: MTM79 is an 80 to 180°C (176 to 356°F) curing epoxy matrix for the manufacture of components operating at high service temperatures. MTM79 has been developed specifically for motorsport bodywork applications.

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage life at -18°C (0°F)
  • Bonds directly to Nomex core in bodywork type applications
  • Excellent tack and drape characteristics
  • High service temperature, ultimate Tg of 220°C (428°F)
  • Flexible curing, 80 to 180°C (176 to 356°F)
Property data reported for dry samples after cure cycle: 1.5 hrs at 135°C (275°F), 6.2 bar (90 psi)+2 hrs at 180°C (356°F). Data normalized to 41 vol% except for shear properties.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, Unreinforced cured resin
  • Storage Temperature
  • Tensile Strength, ASTM D3039, 90°
  • Tensile Strength, ASTM D3039, 0°
  • Elongation at Break, ASTM D3039, 90° Tensile
  • Elongation at Break, ASTM D3039, 0° Tensile
  • Elongation at Break, SACMA SRM01R94, 0° Compression
  • Elongation at Break, SACMA SRM01R94, 90° Compression
  • Tensile Modulus, ASTM D3039, 0°
  • Tensile Modulus, ASTM D3039, 90°
  • Compressive Strength, SACMA SRM01R94, 90°
  • Compressive Strength, SACMA SRM01R94, 0°
  • Compressive Modulus, SACMA SRM01R94, 0°
  • Compressive Modulus, SACMA SRM01R94, 90°
  • Poissons Ratio, SACMA SRM01R94, 90° Compression
  • Poissons Ratio, SACMA SRM01R94, 0° Compression
  • Poissons Ratio, ASTM D3039, 0° Tensile
  • Poissons Ratio, ASTM D3039, 90° Tensile
  • Shear Modulus, ASTM D3518, In-plane
  • Shear Strength, ASTM D2344, 0° Interlaminar
  • Shear Strength, ASTM D3518, In-plane
  • Glass Transition Temp, Tg, DMA E' onset Tg, 16 hrs at 80°C
  • Glass Transition Temp, Tg, DMA E' onset Tg, wet
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1.5 hrs at 135°C
  • Glass Transition Temp, Tg, DMA E' onset Tg, dry
  • Processing Temperature, Alternate Cure
  • Processing Temperature, Recommended Cure
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.