| CirculenRenew C14 HP456J is part of the Circulen© product family of circular and sustainable solutions. CirculenRenew C14 polymer reduces the carbon footprint as it replaces fossil feedstock through using renewable raw materials made from bio-based waste and residue oils. The renewable content of CirculenRenew C14 is measured by an accredited third party laboratory and stated as a parameter on the Certificate of Analysis (CoA). CirculenRenew C14 HP456J is a drop-in solution and therefore doesn’t require any adaptation of the existing processing equipment. CirculenRenew C14 HP456J is a polypropylene homopolymer used for extrusion and thermoforming applications. CirculenRenew C14 HP456J is formulated with a low water-carry-over additive package. Typical applications are monofilaments, ropes, tapes and films. Status: Commercial - Active Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; South & Central America Application: Cast Stretch Film; General Purpose Film Packaging; Raffia/Tapes/Strapping; Strapping Market: Textile Processing Method: Tapes & Raffia Attribute: Homopolymer Information provided by LyondellBasell. |